ML20148D685

From kanterella
Jump to navigation Jump to search
Informs of Delay of Implementation of 881221 Suggestion Re Limiting Waste Loadings of Bead Resin Waste Formulations to 18 Weight Percent.Reasons for Delay Based on Resin Test Results & Effect of Cure Time
ML20148D685
Person / Time
Issue date: 01/11/1988
From: Voit R
LN TECHNOLOGIES CORP. (FORMERLY LONDON NUCLEAR SVCS
To: Tokar M
NRC OFFICE OF NUCLEAR MATERIAL SAFETY & SAFEGUARDS (NMSS)
References
REF-WM-20 LN-87-00016-0P2, LN-87-16-P2, NUDOCS 8803240165
Download: ML20148D685 (2)