Start date | Site | Title | |
---|---|---|---|
ENS 51742 | 16 February 2016 11:31:00 | Hatch | Weld Overlay Flaw Did Not Meet Acceptance Criteria |
ENS 48998 | 3 May 2013 04:00:00 | Wollaston Alloys, Inc. | Part 21 Report - Insufficient Process Control on Pump Impeller |
ENS 47767 | 24 March 2012 22:55:00 | North Anna | Degradation of Steam Generator Nozzle Weld Areas |
ENS 44102 | 27 March 2008 20:45:00 | Brunswick | Unacceptable Flaw Found in Rpv Cap to Pipe Weld |
ENS 44037 | 6 March 2008 02:00:00 | Crystal River | Circumferential Piping Crack |
ENS 44005 | 23 February 2008 21:00:00 | Hatch | Unacceptable Flaw in Rpv Cap-To-Pipe Weld |
ENS 43880 | 4 January 2008 07:50:00 | Davis Besse | Pressure Boundary Leakage Discovered During Refueling |
ENS 43322 | 26 April 2007 23:30:00 | Pilgrim | Degraded Condition During Weld Deposit Overlay Repair |
ENS 42897 | 11 October 2006 17:40:00 | Wolf Creek | Unanalyzed Condition - Indications on Pressurizer Nozzle to Safe End Welds |
ENS 42059 | 18 October 2005 13:30:00 | Millstone | Ut Examination Discovered an Unacceptable Spray Line to Pressurizer Weld |
ENS 41445 | 26 February 2005 20:30:00 | Calvert Cliffs | Degraded Condition of Reactor Coolant Boundary Weld |